Material Notes:
Volatile silicone, decamethylcyclopentasiloxane (Cyclomethicone NF) for use in a wide range of skincare and topical pharmaceutical delivery applications.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc

@Temperature 25.0 °C
0.950 g/cc

@Temperature 77.0 °F
Viscosity Measure 4.0 cSt
4.0 cSt
Kinetic/Kinematic
Surface Tension 18 dynes/cm
18 dynes/cm
Thermal Properties Metric English Comments
Melting Point <= -50.0 °C
<= -58.0 °F
Boiling Point 205 °C
401 °F
Flash Point 77.0 °C
171 °F
Closed cup
Optical Properties Metric English Comments
Refractive Index 1.397
1.397
Descriptive Properties Value Comments
Cyclotetrasiloxane Content (%) <1