Thermal Properties Metric English Comments
Thermal Conductivity 0.278 W/m-K

@Temperature 982 °C
1.93 BTU-in/hr-ft²-°F

@Temperature 1800 °F
Mid-Mountain Materials CERMEX® MT1800 Needled Silica Mat
CERMEX® MT1800 Needled Silica Blanket is a binderless material comprised of high purity, amorphous silica fibers. In demanding applications, the abrasion and vibration resistance of this mat make..