Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thickness = 500 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness <= 12700 microns
<= 500 mil
Cured film
Resin Technology Group UV-412 Medium Viscosity, High Clarity, UV Curable Adhesive
UV 412 is a high clarity, fast setting UV adhesive. This solvent free adhesive is designed to bond a wide variety of transparent materials, (similar and dissimilar substrates). The high clarity prov..
Thickness 12700 microns
500 mil
Mid-Mountain Materials CERMEX® MT1000 Needled Fiberglass Mat
CERMEX® MT1000 fiberglass mat is comprised of high purity, highly resilient E-Glass fibers. CERMEX® MT1000 is lightweight, strong, and highly efficient as insulation in most high heat environm..
Thickness 12700 microns
500 mil
Mid-Mountain Materials CERMEX® MT1800 Needled Silica Mat
CERMEX® MT1800 Needled Silica Blanket is a binderless material comprised of high purity, amorphous silica fibers. In demanding applications, the abrasion and vibration resistance of this mat make..
Thickness 12700 microns
500 mil
Unifrax FyreWrap® 0.5 Plenum Insulation
Unifrax's FyreWrap® 0.5 Plenum Insulation is a high-temperature insulation blanket specifically designed to provide a single layer, flexible enclosure around combustible items located within fire-r..
Copyright © lookpolymers.com All Rights Reserved