Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.278 W/m-K @Temperature 982 °C |
1.93 BTU-in/hr-ft²-°F @Temperature 1800 °F |
|
Mid-Mountain Materials CERMEX® MT1800 Needled Silica Mat CERMEX® MT1800 Needled Silica Blanket is a binderless material comprised of high purity, amorphous silica fibers. In demanding applications, the abrasion and vibration resistance of this mat make.. |