Physical Properties | Metric | English | Comments |
---|---|---|---|
Filament Diameter | 6.0 - 9.0 µm | 6.0 - 9.0 µm | |
Mid-Mountain Materials CERMEX® MT1800 Needled Silica Mat CERMEX® MT1800 Needled Silica Blanket is a binderless material comprised of high purity, amorphous silica fibers. In demanding applications, the abrasion and vibration resistance of this mat make.. |
|||
Filament Diameter | 6.0 - 9.0 µm | 6.0 - 9.0 µm | |
Zircar Refractory Composites SB-2000 SILICA BLANKET ZIRCAR Silica Blanket Type SB-2000 is a high temperature insulation blanket made of mechanically interlocked continuous filament amorphous silica fibers with useful properties to temperatures of 110.. |