Material Notes:
Used for microdermabrasion. Dermagrain is a specially graded high purity micro crystalline aluminum oxide made from Bayer process alumina which results in final product purity of 99.55%. It has been fused at nearly 4000°F to make an extremely stable material with the identical crystal structure of sapphire. Aluminum oxide is completely inert and pH neutral. Components made from aluminum oxide are approved for use by the FDA as prosthetic and dental implants.After fusion the material is processed to form grains with blocky, sharp edges to enhance abrasive properties. It is then graded into a tightly controlled particle size distribution. Close examination under a microscope will show that the individual particles are clear grains of sapphire and will sparkle like diamond under reflected light. Because they are clear and absorb light, the grains appear slightly off white in color. Dermagrain 1200 has a D50 (median) particle diameter of 100 microns.Data provided by the supplier, MarkeTech International.
Physical Properties Metric English Comments
Density 3.95 g/cc
0.143 lb/in³
Apparent Bulk Density 1.64 - 1.72 g/cc
0.0592 - 0.0621 lb/in³
Mechanical Properties Metric English Comments
Knoop Microhardness 2000
2000
Knoop 100 Hardness
Hardness, Mohs 9.0
9.0
Thermal Properties Metric English Comments
Melting Point 2022 °C
3672 °F
Component Elements Properties Metric English Comments
Al2O3 99.55 %
99.55 %
Alkalis 0.30 %
0.30 %
CaO 0.030 %
0.030 %
Fe2O3 0.040 %
0.040 %
MgO 0.020 %
0.020 %
SiO2 0.050 %
0.050 %
TiO2 0.010 %
0.010 %
Descriptive Properties Value Comments
Color Off White