Polymer Property : Melting Point = 3672 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 2022 °C
3672 °F
MarkeTech Dermagrain 1200 Microcrystalline Alumina for Microdermabrasion
Used for microdermabrasion. Dermagrain is a specially graded high purity micro crystalline aluminum oxide made from Bayer process alumina which results in final product purity of 99.55%. It has be..