Physical Properties Metric English Comments
Apparent Bulk Density 1.64 - 1.72 g/cc
0.0592 - 0.0621 lb/in³
MarkeTech Dermagrain 1200 Microcrystalline Alumina for Microdermabrasion
Used for microdermabrasion. Dermagrain is a specially graded high purity micro crystalline aluminum oxide made from Bayer process alumina which results in final product purity of 99.55%. It has be..