Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 3.96 g/cc | 0.143 lb/in³ | Sintered Density |
Nabaltec NABALOX® NO 713-40 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 3.96 g/cc | 0.143 lb/in³ | |
Ferro IX 2443 Passivation Glasses - High Voltage (Zn-B-Silicates) Typical Powder Form: RWG, DSD Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures a.. |
|||
Density | 3.97 g/cc | 0.143 lb/in³ | |
MarkeTech Aluminum Oxide Ceramic - Alumina 96% Data provided by the supplier, MarkeTech International.Because of their high temperature, chemical, electrical, and mechanical properties along with their relatively low cost and ease of manufacture.. |
|||
Density | 3.97 g/cc | 0.143 lb/in³ | |
MarkeTech Aluminum Oxide Ceramic - Alumina 97.5% Data provided by the supplier, MarkeTech International.Because of their high temperature, chemical, electrical, and mechanical properties along with their relatively low cost and ease of manufacture.. |
|||
Density | 3.97 g/cc | 0.143 lb/in³ | |
MarkeTech Aluminum Oxide Ceramic - Alumina 98% Data provided by the supplier, MarkeTech International.Because of their high temperature, chemical, electrical, and mechanical properties along with their relatively low cost and ease of manufacture.. |
|||
Density | 3.97 g/cc | 0.143 lb/in³ | |
MarkeTech Aluminum Oxide Ceramic - Alumina 99.5% Data provided by the supplier, MarkeTech International.Because of their high temperature, chemical, electrical, and mechanical properties along with their relatively low cost and ease of manufacture.. |
|||
Density | 3.95 g/cc | 0.143 lb/in³ | |
MarkeTech Dermagrain 1200 Microcrystalline Alumina for Microdermabrasion Used for microdermabrasion. Dermagrain is a specially graded high purity micro crystalline aluminum oxide made from Bayer process alumina which results in final product purity of 99.55%. It has be.. |
|||
Density | 3.96 g/cc | 0.143 lb/in³ | |
ICE Al2O3 94 Data provided by the manufacturer, International Ceramic Engineering. |
|||
Density | 3.96 g/cc | 0.143 lb/in³ | |
ICE Al2O3 96 Data provided by the manufacturer, International Ceramic Engineering. |
|||
Density | 3.97 g/cc | 0.143 lb/in³ | |
Sapco 99.9% Aluminum Oxide Information provided by Sapco. |
|||
Density | 3.96 g/cc | 0.143 lb/in³ | DIN EN 623-2 |
CeramTec RK 87 Alumina, 99.8% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Density | 3.95 g/cc | 0.143 lb/in³ | ASTM-C373 |
CoorsTek Superstrate® TPS 99.6% Alumina Thin Film Applications: thin film substrates |
|||
Density | 3.95 g/cc | 0.143 lb/in³ | DIN EN 623-2 |
CeramTec AT 79 Alumina, 99.6% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |