Material Notes:
A high viscosity resin for blow molding as well as injection molding heavy wall parts requiring maximum impact strength. Also available: P1083, same with UV stabilizer; P1081R, same with release; P1083R, with UV and release; P1084, FDA approved.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
ASTM D570
Moisture Absorption at Equilibrium 0.35 %
0.35 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 3.0 - 4.0 g/10 min
3.0 - 4.0 g/10 min
Cond. O
Mechanical Properties Metric English Comments
Hardness, Rockwell M 70
70
ASTM D785
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Ultimate 66.0 MPa
9570 psi
ATSM D638
Elongation at Break 125 %
125 %
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 2.30 GPa
334 ksi
ASTM D790
Izod Impact, Notched 8.00 J/cm
15.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 142 °C
288 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
ASTM D648