MetalTek MTEK WC 1 UNS J13047 Cast Alloy Steel

Category Metal , Ferrous Metal , Alloy Steel , AISI 8000 Series Steel
Manufacturer MetalTek
Trade Name MTEK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK WC 1 UNS J13047 Cast Alloy Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General structural use.Applications: Cylinders, rolls, hollow shafts.Information provided by MetalTek
Mechanical Properties Metric English Comments
Hardness, Brinell 197
197
Tensile Strength, Ultimate >= 450 MPa
>= 65300 psi
Tensile Strength, Yield >= 240 MPa
>= 34800 psi
Elongation at Break >= 24 %
>= 24 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.25 %
<= 0.25 %
Iron, Fe 97.7 - 99.05 %
97.7 - 99.05 %
As Balance
Manganese, Mn 0.50 - 0.80 %
0.50 - 0.80 %
Molybdenum, Mo 0.45 - 0.65 %
0.45 - 0.65 %
Silicon, Si <= 0.60 %
<= 0.60 %
Descriptive Properties Value Comments
Heat Treatment Quench & Temper