Material Notes:
• For extrusion applications• Excellent process ability.Information provided by MRC Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ISO 1183
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Ash <= 1.0 %
<= 1.0 %
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength 27.9 MPa
4050 psi
ISO 527
Elongation at Break 84 %
84 %
ISO 527
Flexural Strength 29.0 MPa
4210 psi
ISO 178
Flexural Modulus 0.979 GPa
142 ksi
ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.3 °C
186 °F
ISO 75