Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | <= 29.0 MPa | <= 4210 psi | ISO 178 |
Polykemi AB POLYfill PPC T1010 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 29.0 MPa | 4200 psi | ASTM D790 |
Quadrant EPP TIVAR® MD UHMW-PE, FDA Metal Detectable (ASTM Product Data Sheet) Meets FDA and USDA guidelines; 3-A Dairy-approved (natural) Reduces noise Self-lubricating Chemical-, corrosion- and wear-resistant No moisture absorption Non-toxic, low-friction surface Meets ASTM.. |
|||
Flexural Strength | 29.0 MPa | 4200 psi | ASTM D790 |
Network Polymers 702 Polystyrene Description: Ignition RetardantInformation provided by Network Polymers Inc. |
|||
Flexural Strength | 29.0 MPa | 4200 psi | ASTM D790 |
Fiberfil® PP-61/CC/20 Polypropylene Copolymer, 20% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 29.0 MPa | 4200 psi | ASTM D790 |
Fiberfil® PP-62/CC/20/UV Polypropylene Copolymer, 20% Calcium Carbonate, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 29.0 MPa | 4210 psi | ASTM D790 |
LG Chemical LUPOL SO-5202P High Impact Polypropylene, 20% Polymer Alloy LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Flexural Strength | 29.0 MPa | 4210 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP (Asia Pacific) LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 29.0 MPa | 4200 psi | ASTM D790 |
Techmer ES Statiblend® 02020 MB Polypropylene, 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 5% Filler by Weight/Unspecified FillerReinforFeatures: ConductiveTPCI# 9117116Information provided by TP Composites, Inc. |
|||
Flexural Strength | 29.0 MPa | 4210 psi | ASTM D790 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 29.0 MPa | 4210 psi | ASTM D790 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 29.0 MPa | 4210 psi | ASTM D790 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 29.0 MPa | 4210 psi | ASTM D790 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 29.0 MPa | 4210 psi | ASTM D790 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 29.0 MPa | 4210 psi | ASTM D790 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Flexural Strength | 29.0 MPa | 4200 psi | ASTM D790 |
Ensinger Tecatron® XP-76 Compression Molded PPS Compound, 55% PTFE Filled Seal Material Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Flexural Strength | 29.0 MPa | 4210 psi | ASTM D790 |
Entec Hypro™ PPC-CC10 Natural Copolymer Polypropylene, 10% Calcium Carbonate Filled Information provided by Entec |
|||
Flexural Strength | >= 29.0 MPa | >= 4210 psi | high temp bending |
China-Yixing Longly Refractories Load Bearing Board Corundum-Mullite Products with high-purity fused alumina and fused mullite for raw materials, the use of high-tonnage press repression, from ultra-high-temperature sintering; high-purity, the main phase (or corundum.. |
|||
Flexural Strength | 29.0 MPa | 4210 psi | ASTM D790 |
Aclo Accucomp Polypropylene CPO406L Copolymer |
|||
Flexural Strength | 29.0 MPa | 4210 psi | ISO Data |
BASF Ultramid® 8202CQ PA6 (Conditioned) Ultramid 8202CQ is a low viscosity, PA6 injection molding homopolymer, possessing a modified crystalline structure or increased property performance and faster cycles. It is also available in pigme.. |
|||
Flexural Strength | 29.0 MPa | 4200 psi | ASTM D790 |
Americas Styrenics EA6740 High Impact Polystyrene Product CharacteristicsVery good printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsPackaging and one-time use it.. |
|||
Flexural Strength | 29.0 MPa | 4210 psi | ASTM D790 |
Aclo Accutech Polyethylene HD0234G10UVL High Density Glass Reinforced UV Stabilized |
|||
Flexural Strength | 29.0 MPa | 4210 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436T10L1 Talc Reinforced |
|||
Flexural Strength | 29.0 MPa | 4210 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436T40L Talc Reinforced |
|||
Flexural Strength | 29.0 MPa | 4210 psi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 152 Polypropylene, Mineral Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.20% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Flexural Strength | 29.0 MPa | 4210 psi | ISO 178 |
MRC Polymers MAXTEL™ 630-BK Polypropylene Copolymer • For extrusion applications• Excellent process ability.Information provided by MRC Polymers Inc. |
|||
Flexural Strength | 29.0 MPa | 4210 psi | ASTM D790 |
Lucent Polymers TPO-10T Thermoplastic Polyolefin, 10% Mineral Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Flexural Strength | 29.0 MPa | 4210 psi | ASTM D790 |
Aclo Accutech TPO TPO030T9V Paintable Grade Approved to Suzuki Spec Black B14257 |