M. Holland Company LL800 LLDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company LL800 LLDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Fast Production Cycle, High Gloss, Low Temp. Impact Resistance, Low to No Odor, Low WarpageUses: Containers, Household Goods, Lids, Thin-walled PartsApprovals: FDA 21 CFR 177.1520(c) 3.2a Processing Method: Injection MoldingInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.929 g/cc
0.0336 lb/in³
ASTM D792
Melt Flow 55 g/10 min

@Load 2.16 kg,
Temperature 190 °C
55 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 56
56
ASTM D2240
Tensile Strength, Yield 16.5 MPa
2400 psi
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
Flexural Modulus 0.469 GPa
68.0 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 100 °C
212 °F
ASTM D1525
Descriptive Properties Value Comments
Form Pellets