Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.469 GPa | 68.0 ksi | ASTM D790 |
M. Holland Company LL800 LLDPE
(discontinued **) Features: Fast Production Cycle, High Gloss, Low Temp. Impact Resistance, Low to No Odor, Low WarpageUses: Containers, Household Goods, Lids, Thin-walled PartsApprovals: FDA 21 CFR 177.1520(c) 3.2a .. |
|||
Flexural Modulus | 0.469 GPa | 68.0 ksi | ASTM D790 |
Multibase Multi-Flex® D 4502 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot.. |
|||
Flexural Modulus | 0.469 - 0.689 GPa | 68.0 - 100 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6 IM 435 HS L Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedUses: Low Temperature ApplicationsInformatio.. |
|||
Flexural Modulus | 0.469 - 20.0 GPa | 68.0 - 2900 ksi | Average value: 4.97 GPa Grade Count:236 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Flexural Modulus | 0.469 GPa | 68.0 ksi | 1% Secant, 0.05 in/min; ASTM D790 |
LyondellBasell Hifax™ CA207A Thermoplastic Polyolefin Elastomer Description: Hifax™ CA207A thermoplastic olefin resin is designed to reduce shrinkage and improve paint adhesion of PP compound. It is based on proprietary Basell process technology. All ingredien.. |