Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

M Chemical GUARD DOGâ„¢ UV9 Light Stabilizer, Benzophenone Derivative

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer M Chemical Company, Inc.
Trade Name GUARD DOG™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M Chemical GUARD DOGâ„¢ UV9 Light Stabilizer, Benzophenone Derivative.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GUARD DOG™ UV9 light stabilizer is a derivative of Benzophenone that has an exceptionally strong and broad-range of UV absorption properties (UV A 315 -400 nm and UV B 290 - 314 nm) throughout the UV spectrum. It is a highly efficient UV absorber and is recommended for thermoset plastics and coatings that function as ultraviolet screens for photosensitive substrates. It is stable to heat and light and does not decompose below 200°C.Applications: Extremely effective in PS, rigid and flexible PVC, Thermoset polyester, PMMA, short, medium and long chain alkyds, phenolic and other solvent based systems.Performance Benefits:Highly effective and efficient UV absorber with minimal color contributionIdeal for use in coatings, PVC and thermoset polyester systems.Excellent compatibility with polymers and other stabilizer chemistriesTypical Properties:This product is a pale yellow crystalline powder, freely soluble in most organic solvents and is not soluble in water.Solubility (g/100g @ 25°C): Benzene 128, 95% Ethanol 6.2, Methylene Chloride 147, Styrene 105
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc

@Temperature 25.0 °C
1.32 g/cc

@Temperature 77.0 °F
Solubility in Water 0.0 %
0.0 %
Particle Size <= 0.328 µm
<= 0.328 µm
Molecular Weight 228.24 g/mol
228.24 g/mol
Thermal Properties Metric English Comments
Melting Point 62.0 - 65.0 °C
144 - 149 °F
Descriptive Properties Value Comments
CAS Number 131-57-7
FDA complies
Section 177.1010 - for use in contact with food
Molecular Formula C14H12O3
Name 2-hydroxy-4-methoxybenzophenone
Recommended Dosage 0.1 - 0.5%
in total polymer
Copyright © lookpolymers.com All Rights Reserved