A. Schulman POLYBLAK™ 3422 Black Color Concentrate, 35% Carbon Black Based In LDPE

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYBLAK™ 3422 Black Color Concentrate, 35% Carbon Black Based In LDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPOLYBLAK® Black 3422 is a black color concentrate containing 35% carbon black based in LDPE. This masterbatch is designed to provide excellent UV absorption with a regular brown undertone and pigment particle size of 19 nanometers. POLYBLAK® Black 3422 is specially formulated for use in automotive polypropylene and compounding and injection molding applications. POLYBLAK® Black 3422 is typically recommended for use at 5% addition levels.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Carbon Black Loading 35 %
35 %
Descriptive Properties Value Comments
Moisture (max) 1000
ppm, ASTM D789