Polymer Property : Melting Point = 65.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 62.0 - 65.0 °C
144 - 149 °F
M Chemical GUARD DOGâ„¢ UV9 Light Stabilizer, Benzophenone Derivative
GUARD DOGâ„¢ UV9 light stabilizer is a derivative of Benzophenone that has an exceptionally strong and broad-range of UV absorption properties (UV A 315 -400 nm and UV B 290 - 314 nm) throughout ..
Melting Point 55.0 - 65.0 °C
131 - 149 °F
Fine Organics FINALUX G 121 Lubricant Additive
Applications: Lubricant for rigid PVC fittings, films and other Sn-mercaptide stabilized articles. Suitable for PVC cable compounds.Information provided by Fine Organics
Melting Point 55.0 - 65.0 °C
131 - 149 °F
Fine Organics FINALUX G 321 Lubricant Additive
Applications: All round lubricant for rigid PVC profiles/extrusion and injection molding, lubricant for Polycarbonate.Information provided by Fine Organics
Melting Point 55.0 - 65.0 °C
131 - 149 °F
Fine Organics FINALUX G2 Lubricant Additive
Applications:Intermediate lubricant for:rigid PVC pipesconduitsfootwearcable compoundsInformation provided by Fine Organics
Melting Point 57.0 - 65.0 °C
135 - 149 °F
Indium Corp. Indalloy 140 Bismuth Solder Alloy
Information Provided by Indium Corporation
Melting Point 61.0 - 65.0 °C
142 - 149 °F
Indium Corp. Indalloy 147 Bismuth Solder Alloy
Information Provided by Indium Corporation
Melting Point 60.0 - 65.0 °C
140 - 149 °F
RP-0815
Solvay ALKAMIDE® C 212 Surfactant
INCI NAME: Cocamide MEACAS: 68140-00-1Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: ALKAMIDE C-212 is a versatile and effective alkanolamide for use in soap or syn..
Melting Point 60.0 - 65.0 °C
140 - 149 °F
Aquabond Technologies Aquabond™ ABS-65 Water Soluble Adhesive and Bonding Thermoplastic
Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding tem..