Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 62.0 - 107 °C | 144 - 225 °F | Average value: 83.7 °C Grade Count:22 |
Overview of materials for EMAAA Terpolymer This property data is a summary of similar materials in the MatWeb database for the category "EMAAA Terpolymer". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Melting Point | 62.0 °C | 144 °F | Exxon Method |
ExxonMobil Escorene® MV-02528 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 27.5% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Melting Point | 62.0 - 65.0 °C | 144 - 149 °F | |
M Chemical GUARD DOGâ„¢ UV9 Light Stabilizer, Benzophenone Derivative GUARD DOGâ„¢ UV9 light stabilizer is a derivative of Benzophenone that has an exceptionally strong and broad-range of UV absorption properties (UV A 315 -400 nm and UV B 290 - 314 nm) throughout .. |
|||
Melting Point | 62.0 °C | 144 °F | Eutectic |
Indium Corp. Indalloy 18 Indium Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 62.0 °C | 144 °F | |
Solvay Chemicals Ethyl 3-(difluoromethyl)-1-methyl-1H-pyrazole-4-carboxylate CAS-No.: 141573-95-7 / EC-No.: 619-510-5 Uses: Chemical intermediateInformation provided by Solvay |
|||
Melting Point | 62.0 °C | 144 °F | ASTM D3418 - ISO 3146 |
DuPont Elvaloy® HP661 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |
|||
Melting Point | 62.0 °C | 144 °F | ASTM D3418 - ISO 3146 |
DuPont Elvaloy® HP662 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |
|||
Melting Point | 62.0 °C | 144 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 2022 Acid-Modified Ethylene Terpolymer Adhesive Resin Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Melting Point | 62.0 °C | 144 °F | Freezing Point; ASTM D3418, ISO 3146 |
DuPont™ Surlyn® E185SB Ionomer Resin Surlyn® E185SB is an ionomer of an acid copolymer resin. It is designed for coextrusion with high-density polyethylene in peelable seals applications. It can be used in extrusion equipment designed.. |
|||
Melting Point | 62.0 °C | 144 °F | DSC, 10°C/min (peak); DuPont Test |
Dow Engage® ENR 7270.00 Ethylene-Butene Copolymer Description: ENR 7270.00 is a general purpose ethylene-butene copolymer designed to provide good cost/performance balance in polymer modification applications.Information provided by manufacturer.Th.. |
|||
Melting Point | 62.0 °C | 144 °F | DSC |
Arkema Group EVATANE® 33-45 Copolymer Ethylene - Vinyl Acetate EVATANE® 33-45 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-45 is stabilized with antioxidants. The High Vinyl Acetate co.. |
|||
Melting Point | 62.0 °C | 144 °F | DSC |
Arkema Group LOTADER® 4603 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 4603 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure process in autoclave reactor. LOTADER 4603 is a multipurpose extrusion adhesive used.. |
|||
Melting Point | 62.0 °C | 144 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 2169 Anhydride-Modified Ethylene Acrylate Adhesive Resin
(discontinued **) Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in.. |
|||
Melting Point | 62.0 °C | 144 °F | ASTM D3418 - ISO 3146 |
DuPont Elvaloy® HP663 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer
(discontinued **) Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |