LyondellBasell Lupolen® V 2520 J Ethylene Vinyl Acetate, Film Grade

Category Polymer , Film , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Manufacturer LyondellBasell
Trade Name Lupolen®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Lupolen® V 2520 J Ethylene Vinyl Acetate, Film Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell.
Physical Properties Metric English Comments
Density 0.926 g/cc
0.0335 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 9.00 MPa
1310 psi
Elongation at Break >= 50 %
>= 50 %
Tensile Modulus 0.190 GPa
27.6 ksi
Thermal Properties Metric English Comments
Melting Point 108 °C
226 °F
Flammability, UL94 HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Comparative Tracking Index 600 V
600 V