Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Hifaxâ„¢ CB285 Thermoplastic Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO) , Polyolefin
Manufacturer LyondellBasell
Trade Name Hifax™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Hifaxâ„¢ CB285 Thermoplastic Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Hifaxâ„¢ CB285 high melt flow, 1,300 MPa flexural modulus, low CLTE, UV-stabilized, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of impact resistance, rigidity and dimensional stability. It was designed for exterior ornamentation applications that require stiffness, low thermal expansion characteristics, and good molded part aesthetics. Features include: excellent impact/stiffness balance, excellent molded part aesthetics, low CLTE, low mold shrinkage, very good dimensional stability, and good paintability and weatherability. Typical applications include: painted and molded-in color body side moldings, and painted and molded-in color rigid claddings and rocker panels. Uses: Automotive applicationsInformation provided by Basell.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ISO 1183
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
ISO 527-1, -2
Elongation at Break 500 %
500 %
ISO 527-1, -2
Elongation at Yield 12 %
12 %
ISO 527-1, -2
Flexural Modulus 1.30 GPa
189 ksi
ISO 178
Izod Impact, Notched (ISO) 36.0 kJ/m²

@Temperature 23.0 °C
17.1 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Dart Drop, Total Energy 25.0 J

@Temperature -30.0 °C
18.4 ft-lb

@Temperature -22.0 °F
Instrumented Energy at Maximum Load, Ductile Failure; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 46.0 µm/m-°C

@Temperature -30.0 - 100 °C
25.6 µin/in-°F

@Temperature -22.0 - 212 °F
ASTM D696
Shrinkage 0.50 %
0.50 %
Tool, 100x150x3.2 mm; Basell Test Method
0.800 %

@Temperature 121 °C,
Time 3600 sec
0.800 %

@Temperature 250 °F,
Time 1.00 hour
Afterbake, 100x150x3.2 mm; Basell Method