Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Alathon® L4903 High Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Alathon® L4903 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsALATHON L 4903 is a high molecular weight high density copolymer with broad dimodal molecular weight distribution. This resin exhibits excellent machine direction tear in an HMW-HD resin as well as low gel levels. Typical applications include trash liners and products requiring incorporating PCR.Regulatory StatusL 4903 meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesSpecific recommendations for processing L 4903 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.Typical Extrusion Conditions: BUR=4.1, Neck Height=8 Die Diameters, 0.5 Mil Film, Melt Temperature- 390-410°F(199-210°C)This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
ASTM D1505
Thickness 12.7 microns
0.500 mil
4:1 BUR; Neck Height = 8 Die Diameters
Melt Flow 0.027 g/10 min
0.027 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 41.0 MPa
5940 psi
ASTM D882
Film Tensile Strength at Yield, TD 33.5 MPa
4860 psi
ASTM D882
Film Elongation at Break, MD 390 %
390 %
ASTM D882
Film Elongation at Break, TD 260 %
260 %
ASTM D882
Dart Drop, Total Energy 2.44 J
1.80 ft-lb
ASTM D3420
Elmendorf Tear Strength MD 20 g
20 g
ASTM D1922
Elmendorf Tear Strength TD 18 g
18 g
ASTM D1922
Film Tensile Strength at Break, MD 65.1 MPa
9440 psi
ASTM D882
Film Tensile Strength at Break, TD 66.7 MPa
9680 psi
ASTM D882
1% Secant Modulus, MD 1150 MPa
167000 psi
ASTM D822
1% Secant Modulus, TD 979 MPa
142000 psi
ASTM D822
Processing Properties Metric English Comments
Melt Temperature 199 - 210 °C
390 - 410 °F
Users viewing this material also viewed the following: