Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 979 MPa | 142000 psi | ASTM D822 |
LyondellBasell Alathon® L4903 High Density Polyethylene ApplicationsALATHON L 4903 is a high molecular weight high density copolymer with broad dimodal molecular weight distribution. This resin exhibits excellent machine direction tear in an HMW-HD resi.. |