Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.027 g/10 min | 0.027 g/10 min | ASTM D1238 |
LyondellBasell Alathon® L4903 High Density Polyethylene ApplicationsALATHON L 4903 is a high molecular weight high density copolymer with broad dimodal molecular weight distribution. This resin exhibits excellent machine direction tear in an HMW-HD resi.. |