Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 1% Secant Modulus, MD = 1150 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 1150 MPa
167000 psi
ASTM D822
LyondellBasell Alathon® L4903 High Density Polyethylene
ApplicationsALATHON L 4903 is a high molecular weight high density copolymer with broad dimodal molecular weight distribution. This resin exhibits excellent machine direction tear in an HMW-HD resi..