Polymer Property : Elmendorf Tear Strength TD = 18 g Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Elmendorf Tear Strength TD 18 g
18 g
ASTM D1922
LyondellBasell Alathon® L4903 High Density Polyethylene
ApplicationsALATHON L 4903 is a high molecular weight high density copolymer with broad dimodal molecular weight distribution. This resin exhibits excellent machine direction tear in an HMW-HD resi..