| Category | Polymer , Thermoplastic , Polyetherimide (PEI) |
| Manufacturer | Lucent Polymers |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Lucent Polymers PEI-100 Polyetherimide, General Purpose.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0060 cm/cm @Thickness 3.17 mm |
0.0060 in/in @Thickness 0.125 in |
1/8" Section |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 102 MPa | 14800 psi | ASTM D638 |
| Elongation at Break | >= 10 % | >= 10 % | ASTM D638 |
| Flexural Strength | 138 MPa | 20000 psi | ASTM D790 |
| Flexural Modulus | 3.103 GPa | 450.1 ksi | ASTM D790 |
| Izod Impact, Notched | 0.320 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
0.599 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 200 °C | 392 °F | ASTM D648 |