Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000346 ohm-cm | 0.00000346 ohm-cm | |
Lucas-Milhaupt BRAZE 541 Silver Based Cadmium Free Filler Metal Characteristics:Braze 541 is an intermediate temperature silver brazing alloy with a rather long, 235EF (130EC) melting range. It has a tendency to liquate (i.e. separate into low and high melting .. |
|||
Electrical Resistivity | 0.00000346 ohm-cm | 0.00000346 ohm-cm | |
Lucas-Milhaupt Silvaloy® A54N Brazing Alloy Silvaloy A54N is a silver brazing alloy suitable for furnace brazing due to its low zinc content. Its broader melting range is helpful where clearances are not uniform. During melting, Silvaloy A54N.. |