Polymer Property : Density = 9.62 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 9.62 g/cc
0.348 lb/in³
Lucas-Milhaupt Silvaloy® A54N Brazing Alloy
Silvaloy A54N is a silver brazing alloy suitable for furnace brazing due to its low zinc content. Its broader melting range is helpful where clearances are not uniform. During melting, Silvaloy A54N..