Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 677 - 857.2 °C | 1250 - 1575 °F | |
Lucas-Milhaupt BRAZE 250 Silver Based Cadmium Free Filler Metal Characteristics:Braze 250 is an intermediate temperature silver brazing alloy with a long (325EF/180EC) melting range. It has a tendency to liquate (i.e. separate into low and high melting constitu.. |
|||
Melting Point | 727 - 857.2 °C | 1340 - 1575 °F | |
Lucas-Milhaupt BRAZE 541 Silver Based Cadmium Free Filler Metal Characteristics:Braze 541 is an intermediate temperature silver brazing alloy with a rather long, 235EF (130EC) melting range. It has a tendency to liquate (i.e. separate into low and high melting .. |
|||
Melting Point | 718.3 - 857.2 °C | 1325 - 1575 °F | |
Lucas-Milhaupt Silvaloy® A54N Brazing Alloy Silvaloy A54N is a silver brazing alloy suitable for furnace brazing due to its low zinc content. Its broader melting range is helpful where clearances are not uniform. During melting, Silvaloy A54N.. |
|||
Melting Point | 727 - 857.2 °C | 1340 - 1575 °F | |
Universal Wire Works BAg-13 (AMS 4772) Silver Brazing Filler Metal Information provided by Universal Wire Works for their line of welding wire and filler metal. |