Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon P3272-10Rxx-P4 0.030" (0.762 mm) Cured Self-Fusing Silicone Tape (Rectangular, Unsupported)

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon P3272-10Rxx-P4 0.030" (0.762 mm) Cured Self-Fusing Silicone Tape (Rectangular, Unsupported).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: High strength self-fusing silicone tapeDesign/Construction: Interleave: PolyethyleneRubber: Cured Self-Fusing Silicone Rubber Cross-Section: 1” wide RectangularAppearance: Red silicone rubber on polymer linerAppearance: Red silicone rubber on polymer linerAdvatages:Flexibility: Silicone rubber resists damage due to vibration, frame movement under load and thermal expansion/contraction in use. Silicone based insulation remains flexible even after many years in extreme service conditions.Thermal Stability: Silicone based insulation remains flexible and resilient to thermal shock, even after years of cold motor starts as low as -54°C and running conditions up to 260°C.Electrical Insulation: Silicone based insulation has excellent dielectric strength, dielectric integrity over a wide temperature range, and resists arc tracking, current leakage, corona damage, and dielectric fatigue.Ozone and Weather Resistance: Unique silicone chemistry resists oxidative embrittlement, damage by ozone and other atmospheric chemicals, and seals against moisture, carbon dust, dirt, and debris.This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
Silicone Property; Arlon SQA-TMS-024
Water Absorption 1.6 %
1.6 %
MIL-I-46852C
Thickness 76.2 microns
3.00 mil
Interleave
762 microns
30.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; ASTM D2240
Tensile Strength 10.3 MPa
1500 psi
Silicone Property; ASTM D412
Elongation at Break 475 %
475 %
Silicone Property; ASTM D412
Peel Strength 0.631 kN/m
3.60 pli
Bond Strength; MIL-I-46852C
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 22.4 kV/mm
570 kV/in
ASTM D149
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 23.9 °C
12.0 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Allis-Chalmers Tack 1/16 [in]
Arlon SQA-TMS-013
Color Red