Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 9.63 g/cc | 9.63 g/cc | |
Lucas-Milhaupt Silvaloy® A54N Brazing Alloy Silvaloy A54N is a silver brazing alloy suitable for furnace brazing due to its low zinc content. Its broader melting range is helpful where clearances are not uniform. During melting, Silvaloy A54N.. |