Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loxim 120 01V0 Polycarbonate, 20% Glass Filled, Flame Retardant

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 20% Glass Filled , Polycarbonate, Glass Fiber Filled, Flame Retardant
Manufacturer Loxim Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loxim 120 01V0 Polycarbonate, 20% Glass Filled, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D792
Filler Content 20 %
20 %
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 - 95.0 MPa
13100 - 13800 psi
ASTM D683
Elongation at Break >= 3.0 %
>= 3.0 %
ASTM D638
Tensile Modulus 6.00 GPa
870 ksi
ASTM D638
Flexural Modulus 5.50 GPa
798 ksi
ASTM D790
Izod Impact, Notched 0.800 - 1.00 J/cm
1.50 - 1.87 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 145 - 150 °C
293 - 302 °F
ASTM D1525, HDT Method B
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in