Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.32034 - 1.00 J/cm

@Temperature -40.0 - -40.0 °C
0.60013 - 1.87 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.660 J/cm Grade Count:2
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched 0.300 - 1.00 J/cm

@Temperature -40.0 - -29.0 °C
0.562 - 1.87 ft-lb/in

@Temperature -40.0 - -20.2 °F
Average value: 0.565 J/cm Grade Count:9
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Izod Impact, Notched 1.00 - 1.00 J/cm

@Temperature 0.000 - 0.000 °C
1.87 - 1.87 ft-lb/in

@Temperature 32.0 - 32.0 °F
Average value: 0.960 J/cm Grade Count:2
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
Izod Impact, Notched 1.00 - 1.00 J/cm

@Temperature 0.000 - 0.000 °C
1.87 - 1.87 ft-lb/in

@Temperature 32.0 - 32.0 °F
Average value: 0.945 J/cm Grade Count:3
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
Izod Impact, Notched 0.300 - 1.00 J/cm

@Temperature -40.0 - 0.000 °C
0.562 - 1.87 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 0.512 J/cm Grade Count:3
Overview of materials for Polypropylene with 30% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are..
Izod Impact, Notched 0.430 - 1.00 J/cm
0.806 - 1.87 ft-lb/in
Average value: 0.731 J/cm Grade Count:11
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor..
Izod Impact, Notched 0.800 - 1.00 J/cm
1.50 - 1.87 ft-lb/in
ASTM D256
Loxim 120 01V0 Polycarbonate, 20% Glass Filled, Flame Retardant
Information provided by Loxim Industries
Izod Impact, Notched 0.900 - 1.00 J/cm
1.69 - 1.87 ft-lb/in
ASTM D256
Loxim 330 01V0 Nylon 6
Information provided by Loxim Industries
Izod Impact, Notched 0.800 - 1.00 J/cm
1.50 - 1.87 ft-lb/in
ASTM D256
Loxim 811 02T HB Polypropylene Compound, 10% Talc Filled, Flame Retardant
Information provided by Loxim Industries
Izod Impact, Notched 0.800 - 1.00 J/cm
1.50 - 1.87 ft-lb/in
ASTM D256
Loxim 820 01 HBCC Polypropylene Compound, 20% Chemically Coupled, Flame Retardant
Information provided by Loxim Industries