Latrobe Tatmo-Vâ„¢ AISI M7 High Speed Steel

Category Metal , Ferrous Metal , Alloy Steel , Carbon Steel , High Carbon Steel , Tool Steel
Manufacturer Latrobe Steel
Trade Name Tatmo-V™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe Tatmo-Vâ„¢ AISI M7 High Speed Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tatmo-V is an M7 grade high speed steel with superior abrasion resistance because of its high carbon and vanadium content. It is an excellent choice for premium grade tools which require an outstanding balance of red hardness, edge toughness, and wear resistance. Increased tool life of Tatmo-V is noted in the machining of semi-hard, heat treated steel parts.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Mechanical Properties Metric English Comments
Hardness, Rockwell C 42

@Temperature 649 °C
42

@Temperature 1200 °F
65

@Temperature 50.0 °C
65

@Temperature 122 °F
Izod Impact Unnotched 33.2 J
24.5 ft-lb
Oil Quenched at 1204°C; 482°C Temper Temperature
38.0 J
28.0 ft-lb
Oil Quenched at 1204°C; 593°C Temper Temperature
40.7 J
30.0 ft-lb
Oil Quenched at 1204°C; 622°C Temper Temperature
40.7 J
30.0 ft-lb
Oil Quenched at 1177°C; 482°C Temper Temperature
42.0 J
31.0 ft-lb
Oil Quenched at 1177°C; 593°C Temper Temperature
46.1 J
34.0 ft-lb
Oil Quenched at 1177°C; 622°C Temper Temperature
Component Elements Properties Metric English Comments
Carbon, C 1.0 %
1.0 %
Chromium, Cr 3.75 %
3.75 %
Iron, Fe 83.1 %
83.1 %
Molybdenum, Mo 8.55 %
8.55 %
Tungsten, W 1.6 %
1.6 %
Vanadium, V 2.0 %
2.0 %