Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Unnotched | 46.1 J | 34.0 ft-lb | Oil Quenched at 1177°C; 622°C Temper Temperature |
Latrobe Crusaderâ„¢ ASTM M3-2 High Speed Steel CRUSADER (M3-2) is a high speed steel with an outstanding balance of red hardness, edge toughness and wear resistance. The additional carbon and vanadium provide good resistance to abrasion and edge.. |
|||
Izod Impact Unnotched | 46.1 J | 34.0 ft-lb | Oil Quenched at 1204°C; 622°C Temper Temperature |
Latrobe Starkâ„¢ ASTM M4 High Speed Steel STARK (M4) is a super high speed steel with very high carbon and vanadium contents for exceptional abrasion resistance. It is well suited for premium cutting tools of all types,
particularly those u.. |
|||
Izod Impact Unnotched | 46.1 J | 34.0 ft-lb | Oil Quenched at 1177°C; 622°C Temper Temperature |
Latrobe Tatmo-Vâ„¢ AISI M7 High Speed Steel Tatmo-V is an M7 grade high speed steel with superior abrasion resistance because of its high carbon and vanadium content. It is an excellent choice for premium grade tools which require an outstan.. |