Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact Unnotched = 30.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Unnotched 40.7 - 67.8 J

@Diameter 30.5 mm
30.0 - 50.0 ft-lb

@Diameter 1.20 in
bar
Meehanite Almanite® W1 Wear and Abrasion Resisting Cast Iron
Type W1 is an austenitic-martensitic white iron characterized by high hardness and relatively good impact strength. Type W1 has a pearlitic matrix.General Meehanite information - Meehanite metal is..
Izod Impact Unnotched 40.7 - 54.2 J

@Diameter 20.3 mm
30.0 - 40.0 ft-lb

@Diameter 0.798 in
Meehanite AQ Flake Graphite Cast Iron
Type AQ is a wear and abrasion resisting iron that is readily machinable as-cast but may be "air-hardened" after machining with minimum risk of cracking or distortion. Type AQ is easily heat treate..
Izod Impact Unnotched 40.7 - 54.2 J

@Diameter 20.3 mm
30.0 - 40.0 ft-lb

@Diameter 0.798 in
Meehanite GM-60 Flake Graphite Cast Iron
Type GM-60 possesses exceptionally high physical properties, including good impact strength and shock resistance. GM-60 responds well to heat treatment and surface hardening. Type GM machines to a..
Izod Impact Unnotched 40.7 J
30.0 ft-lb
Oil Quenched at 1204°C; 482°C Temper Temperature
Latrobe Crusaderâ„¢ ASTM M3-2 High Speed Steel
CRUSADER (M3-2) is a high speed steel with an outstanding balance of red hardness, edge toughness and wear resistance. The additional carbon and vanadium provide good resistance to abrasion and edge..
Izod Impact Unnotched 40.7 J
30.0 ft-lb
Oil Quenched at 1204°C; 622°C Temper Temperature
Latrobe Tatmo-Vâ„¢ AISI M7 High Speed Steel
Tatmo-V is an M7 grade high speed steel with superior abrasion resistance because of its high carbon and vanadium content. It is an excellent choice for premium grade tools which require an outstan..
Izod Impact Unnotched 40.7 J
30.0 ft-lb
Oil Quenched at 1177°C; 482°C Temper Temperature
Latrobe Tatmo-Vâ„¢ AISI M7 High Speed Steel
Tatmo-V is an M7 grade high speed steel with superior abrasion resistance because of its high carbon and vanadium content. It is an excellent choice for premium grade tools which require an outstan..
Izod Impact Unnotched 40.7 J
30.0 ft-lb
Air Cooled from 843°C; 150°C Temper Temperature
Latrobe LSS™ A6 Tool Steel (ASTM A6)
TLS A6 tool steel is a medium-alloy, air-hardening tool steel that is characterized by its ability to be through hardened while using the low austenitizing temperatures which are typically associate..