Mechanical Properties Metric English Comments
Izod Impact Unnotched 38.0 J
28.0 ft-lb
Air Cooled from 1010°C; 593°C Temper Temperature
Latrobe LSSâ„¢ D7 Tool Steel (ASTM D7)
TLS D7 tool steel is a high-carbon, high-chromium air-hardening tool steel that exhibits exceptional wear resistance. The high carbon and vanadium contents result in numerous, hard vanadium carbide ..
Izod Impact Unnotched 38.0 J
28.0 ft-lb
Oil Quenched at 1218°C; 482°C Temper Temperature
Latrobe Tatmoâ„¢ ASTM M1 High Speed Steel
TATMO is an M1-type, general-purpose high speed steel. In comparison with other popular high speed steels, it exhibits excellent toughness and grindability. These factors and its relatively low cost..
Izod Impact Unnotched 38.0 J
28.0 ft-lb
Oil Quenched at 1204°C; 593°C Temper Temperature
Latrobe Tatmo-Vâ„¢ AISI M7 High Speed Steel
Tatmo-V is an M7 grade high speed steel with superior abrasion resistance because of its high carbon and vanadium content. It is an excellent choice for premium grade tools which require an outstan..
Izod Impact Unnotched 38.0 J
28.0 ft-lb
Oil Quenched at 1175°C; 482°C Temper Temperature
Latrobe CM-52â„¢ ASTM M52 High Speed Steel
CM-52 is classified as an intermediate type high speed steel of the molybdenum chromium-vanadium variety. It is recommended for intermediate cutting applications such as commercial twist drills and ..