Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Unnotched | 40.7 - 67.8 J @Diameter 30.5 mm |
30.0 - 50.0 ft-lb @Diameter 1.20 in |
bar |
Meehanite Almanite® W1 Wear and Abrasion Resisting Cast Iron Type W1 is an austenitic-martensitic white iron characterized by high hardness and relatively good impact strength. Type W1 has a pearlitic matrix.General Meehanite information - Meehanite metal is.. |
|||
Izod Impact Unnotched | 40.7 - 54.2 J @Diameter 20.3 mm |
30.0 - 40.0 ft-lb @Diameter 0.798 in |
|
Meehanite AQ Flake Graphite Cast Iron Type AQ is a wear and abrasion resisting iron that is readily machinable as-cast but may be "air-hardened" after machining with minimum risk of cracking or distortion. Type AQ is easily heat treate.. |
|||
Izod Impact Unnotched | 40.7 - 54.2 J @Diameter 20.3 mm |
30.0 - 40.0 ft-lb @Diameter 0.798 in |
|
Meehanite GM-60 Flake Graphite Cast Iron Type GM-60 possesses exceptionally high physical properties, including good impact strength and shock resistance. GM-60 responds well to heat treatment and surface hardening. Type GM machines to a.. |
|||
Izod Impact Unnotched | 40.7 J | 30.0 ft-lb | Oil Quenched at 1204°C; 482°C Temper Temperature |
Latrobe Crusaderâ„¢ ASTM M3-2 High Speed Steel CRUSADER (M3-2) is a high speed steel with an outstanding balance of red hardness, edge toughness and wear resistance. The additional carbon and vanadium provide good resistance to abrasion and edge.. |
|||
Izod Impact Unnotched | 40.7 J | 30.0 ft-lb | Oil Quenched at 1204°C; 622°C Temper Temperature |
Latrobe Tatmo-Vâ„¢ AISI M7 High Speed Steel Tatmo-V is an M7 grade high speed steel with superior abrasion resistance because of its high carbon and vanadium content. It is an excellent choice for premium grade tools which require an outstan.. |
|||
Izod Impact Unnotched | 40.7 J | 30.0 ft-lb | Oil Quenched at 1177°C; 482°C Temper Temperature |
Latrobe Tatmo-Vâ„¢ AISI M7 High Speed Steel Tatmo-V is an M7 grade high speed steel with superior abrasion resistance because of its high carbon and vanadium content. It is an excellent choice for premium grade tools which require an outstan.. |
|||
Izod Impact Unnotched | 40.7 J | 30.0 ft-lb | Air Cooled from 843°C; 150°C Temper Temperature |
Latrobe LSS™ A6 Tool Steel (ASTM A6) TLS A6 tool steel is a medium-alloy, air-hardening tool steel that is characterized by its ability to be through hardened while using the low austenitizing temperatures which are typically associate.. |