Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Unnotched | 38.0 J | 28.0 ft-lb | Air Cooled from 1010°C; 593°C Temper Temperature |
Latrobe LSSâ„¢ D7 Tool Steel (ASTM D7) TLS D7 tool steel is a high-carbon, high-chromium air-hardening tool steel that exhibits exceptional wear resistance. The high carbon and vanadium contents result in numerous, hard vanadium carbide .. |
|||
Izod Impact Unnotched | 38.0 J | 28.0 ft-lb | Oil Quenched at 1218°C; 482°C Temper Temperature |
Latrobe Tatmoâ„¢ ASTM M1 High Speed Steel TATMO is an M1-type, general-purpose high speed steel. In comparison with other popular high speed steels, it exhibits excellent toughness and grindability. These factors and
its relatively low cost.. |
|||
Izod Impact Unnotched | 38.0 J | 28.0 ft-lb | Oil Quenched at 1204°C; 593°C Temper Temperature |
Latrobe Tatmo-Vâ„¢ AISI M7 High Speed Steel Tatmo-V is an M7 grade high speed steel with superior abrasion resistance because of its high carbon and vanadium content. It is an excellent choice for premium grade tools which require an outstan.. |
|||
Izod Impact Unnotched | 38.0 J | 28.0 ft-lb | Oil Quenched at 1175°C; 482°C Temper Temperature |
Latrobe CM-52â„¢ ASTM M52 High Speed Steel CM-52 is classified as an intermediate type high speed steel of the molybdenum chromium-vanadium variety. It is recommended for intermediate cutting applications such as commercial twist drills and .. |