Latrobe DuraTech™ A11 Powder Metal Tool Steel (AISI A11)

Category Metal , Ferrous Metal , Alloy Steel , Carbon Steel , High Carbon Steel , Tool Steel , Air-Hardening Steel
Manufacturer Latrobe Steel
Trade Name DuraTech™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe DuraTech™ A11 Powder Metal Tool Steel (AISI A11).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuraTech A11 powder metal tool steel a versatile air-hardening tool and die steel which provides extremely high wear resistance in combination with relatively high impact toughness. A very large volume of hard vanadium carbides provides the high wear resistance. The good impact toughness is the result of the fine grain size, small carbides, and superior cleanliness of the powder metallurgy (PM) microstructure. DuraTech A11 offers substantially better wear resistance than the high-carbon, high chromium die steels such as D2 and D7.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 7.41 g/cc
7.41 g/cc
Density 7.39 g/cc
0.267 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 63
63
Oil Quenched from 1177°C; 5 minutes
65.0
65.0
Oil Quenched from 1121°C; 20 minutes
65
65
Oil Quenched from 1066°C; 45 minutes
Modulus of Elasticity 221 GPa
32000 ksi
Machinability 35 - 40 %
35 - 40 %
1% Carbon Steel
Thermal Properties Metric English Comments
CTE, linear 10.71 µm/m-°C

@Temperature 21.0 - 100 °C
5.950 µin/in-°F

@Temperature 69.8 - 212 °F
12.31 µm/m-°C

@Temperature 21.0 - 538 °C
6.839 µin/in-°F

@Temperature 69.8 - 1000 °F
Component Elements Properties Metric English Comments
Carbon, C 2.45 %
2.45 %
Chromium, Cr 5.25 %
5.25 %
Iron, Fe 79.75 %
79.75 %
Manganese, Mn 0.50 %
0.50 %
Molybdenum, Mo 1.35 %
1.35 %
Silicon, Si 0.90 %
0.90 %
Vanadium, V 9.8 %
9.8 %
Chemical Properties Metric English Comments
Critical Temperature 838 °C
1540 °F
Ac1
Users viewing this material also viewed the following: