Polymer Property : Modulus of Elasticity = 32000 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 221 GPa
32000 ksi
Latrobe DuraTechâ„¢ NINE Powder Metal Tool Steel
DuraTech NINE is an air-hardening, powder metal tool steel that provides very high wear resistance in combination with high impact toughness. A large volume of hard vanadium carbides provides the hi..
Modulus of Elasticity 221 GPa

@Temperature 399 °C
32000 ksi

@Temperature 750 °F
hardened and tempered
Bohler-Uddeholm UDDEHOLM VANADIS 60 Powder Metallurgically Produced Tool Steel
Uddeholm Vanadis 60 is a high alloyed powder metallurgical high speed steel suitable for very demanding cold work applications and for cutting tools. The high carbon and alloying content, Co, Mo, W ..
Modulus of Elasticity 221 GPa
32000 ksi
California Fine Wire Alloy 422 Precious Metal Alloy
All values may vary dependent on specific design and usageProprietary compositionCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Modulus of Elasticity 221 GPa
32000 ksi
Latrobe DuraTech™ A11 Powder Metal Tool Steel (AISI A11)
DuraTech A11 powder metal tool steel a versatile air-hardening tool and die steel which provides extremely high wear resistance in combination with relatively high impact toughness. A very large vol..