Physical Properties Metric English Comments
Specific Gravity 7.41 g/cc
7.41 g/cc
Latrobe DuraTechâ„¢ NINE Powder Metal Tool Steel
DuraTech NINE is an air-hardening, powder metal tool steel that provides very high wear resistance in combination with high impact toughness. A large volume of hard vanadium carbides provides the hi..
Specific Gravity 7.41 g/cc
7.41 g/cc
Latrobe DuraTech™ A11 Powder Metal Tool Steel (AISI A11)
DuraTech A11 powder metal tool steel a versatile air-hardening tool and die steel which provides extremely high wear resistance in combination with relatively high impact toughness. A very large vol..