Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.39 g/cc | 0.267 lb/in³ | |
Indium Corp. Indalloy 132 Tin Solder Alloy High temperature electrical solderInformation Provided by Indium Corporation |
|||
Density | 7.40 g/cc | 0.267 lb/in³ | |
Indium Corp. Indalloy® 241 95.5Sn/3.8Ag/0.7Cu Lead-Free Solder Alloy Multicore promoted alloy.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 7.40 g/cc | 0.267 lb/in³ | |
Indium Corp. Indalloy® 246 95.5Sn/4.0Ag/0.5Cu Lead-Free Solder Alloy Petzow (German) prior art reference makes this alloy patent-free.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 7.40 g/cc | 0.267 lb/in³ | |
Indium Corp. Indalloy® 252 95.5Sn/3.9Ag/0.6Cu Lead-Free Solder Alloy Alloy of choice for general SMT assembly. NEMI promoted alloy (average composition of Indalloy #241& #246).Information provided by the manufacturer, Indium Corporation. |
|||
Density | 7.40 g/cc | 0.267 lb/in³ | |
Indium Corp. Indalloy® 256 96.5Sn/3.0Ag/0.5Cu Lead-Free Solder Alloy Referred to as the SAC305 alloy.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 7.39 g/cc | 0.267 lb/in³ | |
Lucas-Milhaupt Silvabrite® Lead-Free Solder Silvabrite silver/tin soldering alloys have been engineered specifically for field repair. These silver/tin solders have been specifically formulated to make difficult repairs swiftly and confidentl.. |
|||
Density | 7.39 g/cc | 0.267 lb/in³ | |
Lucas-Milhaupt Silvabrite® S™ Lead-Free Solder Silvabrite silver/tin soldering alloys have been engineered specifically for field repair. These silver/tin solders have been specifically formulated to make difficult repairs swiftly and confidentl.. |
|||
Density | 7.38 g/cc | 0.267 lb/in³ | |
Indium Corp. Indalloy® 290 In-Ag Solder Alloy Indium with silver added to improve strength. Has the wettability and low-temperature malleability of indium. Particularly useful for cryogenic applications.Information provided by the manufacturer,.. |
|||
Density | 7.39 g/cc | 0.267 lb/in³ | |
Latrobe DuraTechâ„¢ NINE Powder Metal Tool Steel DuraTech NINE is an air-hardening, powder metal tool steel that provides very high wear resistance in combination with high impact toughness. A large volume of hard vanadium carbides provides the hi.. |
|||
Density | 7.40 g/cc | 0.267 lb/in³ | |
Sinotek Materials Tungsten Disulfide (WS2) Powder, High-Purity Tungsten Disulfide powder mainly has applications in spraying, coating, carbon material, all sorts of grease, lubricating oil, friction materials and catalysts. Tungsten Disulfide has good resistan.. |
|||
Density | 7.38 g/cc | 0.267 lb/in³ | |
Williams Advanced Alloys WS143 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 7.40 g/cc | 0.267 lb/in³ | |
Goodfellow Nickel/Iron/Silicon/Boron Alloy Metallic glass (glassy alloy) or amorphous metal. Uses include soft magnetic applications, brazing, coating and as reinforcing fibers.Information provided by Goodfellow.Composition Notes: Si + B co.. |
|||
Density | 7.40 g/cc | 0.267 lb/in³ | |
American Elements Europium Oxide Nanopwder General DescriptionEU-MITE powders and dispersions are inorganic europium-oxide nanoparticles. EU-MITE-A products are uncoated and hydrophilic. EU-MITE-O products are coated with an organic silane (.. |
|||
Density | 7.40 g/cc | 0.267 lb/in³ | |
Crucible Steel CPM® S90V® (420V®) Tool Steel CPM S90V is a unique tool steel made by the Crucible Particle Metallurgy process. It is a martensitic stainless steel with a high volume of vanadium carbides for exceptionally good wear resistance. .. |
|||
Density | 7.40 g/cc | 0.267 lb/in³ | |
BryCoat WS2 Tungsten Disulfide Coating WS2's unique, extensively modified lamellar composition of tungsten disulfide results in a high performance dry coating lubricant. A pressurized air application processes impinges a dry metallic co.. |
|||
Density | >= 7.40 g/cc | >= 0.267 lb/in³ | |
Channel Industries 5700 Lead Zirconate Titanate Piezoelectric Navy Type VICharacterized by high coupling factors and high piezoelectric and dielectric constants over extended temperature ranges and stress amplitudes, lead zirconate titanates are the most exten.. |
|||
Density | 7.38 g/cc | 0.267 lb/in³ | |
AIM SAC305 Lead-Free Solder for Photonic Packaging This alloy falls under the JEIDA recommendation for lead-free soldering. When used in wave soldering, AIM’s SAC305 bar solder offers far superior fluidity as compared to other alloys and makes of b.. |
|||
Density | 7.39 g/cc | 0.267 lb/in³ | |
Latrobe DuraTech™ A11 Powder Metal Tool Steel (AISI A11) DuraTech A11 powder metal tool steel a versatile air-hardening tool and die steel which provides extremely high wear resistance in combination with relatively high impact toughness. A very large vol.. |
|||
Density | 7.38 g/cc | 0.267 lb/in³ | |
AIM 97In/3Ag Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Density | 7.40 g/cc | 0.267 lb/in³ | |
Indium Corp. Indalloy 203 Indium Solder Alloy Information Provided by Indium Corporation |