Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Critical Temperature = 1540 °F Product List

Chemical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Chemical Properties Metric English Comments
Critical Temperature 835 °C
1540 °F
Ac1
Latrobe Crusaderâ„¢ ASTM M3-2 High Speed Steel
CRUSADER (M3-2) is a high speed steel with an outstanding balance of red hardness, edge toughness and wear resistance. The additional carbon and vanadium provide good resistance to abrasion and edge..
Critical Temperature 840 °C
1540 °F
Ac1
Latrobe LSSâ„¢ H13 PQ Hot Work Tool Steel
TLS H13 PQ is Premium Quality H13 hot work steel that is designed to meet the highest quality standards in the die casting industry, and to excel in the most demanding hot work tooling applications...
Critical Temperature 840 °C
1540 °F
Ac1
Latrobe LSSâ„¢ H13 Tool Steel (ASTM H13)
TLS H13 tool steel is a versatile chromium-molybdenum hot work steel that is widely used in hot work and cold work tooling applications. The hot hardness (hot strength) of H13 resists thermal fatigu..
Critical Temperature 838 °C
1540 °F
Ac1
Latrobe LSSâ„¢ H19 Hot Work Tool Steel (ASTM H19)
TLS H19 hot work tool steel is a hot work steel that exhibits excellent resistance to softening at elevated temperature. This grade maintains high hardness and resistance to thermal fatigue cracking..
Critical Temperature 840 °C
1540 °F
Ac1
Latrobe Viscount 20® Free Machining Tool Steel (ASTM H13S)
Viscount 20 tool steel is a resulfurized H13 tool steel. The distribution of alloy sulfide particles in the microstructure enhances the machinability of the steel in the annealed condition. In addi..
Critical Temperature 835 °C
1540 °F
Ac1
Latrobe Corsairâ„¢ ASTM M3-1 High Speed Steel
CORSAIR (M3-1) contains carbon and vanadium levels that are intermediate between those of Double Six (M2) and Crusader (M3-2). This gives the steel a fine balance of wear resistance and grindability..
Critical Temperature 840 °C
1540 °F
Ac1
Latrobe DuraTechâ„¢ M4 High Carbon Powder Metal High Speed Steel (ASTM M4)
DuraTech M4 high speed steel is an extremely versatile high speed steel which provides a unique combination of high wear resistance with high impact toughness and transverse bend strength. A large v..
Critical Temperature 840 °C
1540 °F
Ac1
Latrobe DuraTechâ„¢ M4 Powder Metal High Speed Steel (ASTM M4)
DuraTech M4 high speed steel is an extremely versatile high speed steel which provides a unique combination of high wear resistance with high impact toughness and transverse bend strength. A large v..
Critical Temperature 835 °C
1540 °F
Ac1
Latrobe DuraTechâ„¢ M48 Powder Metal High Speed Steel (ASTM M48)
DuraTech M48 super high speed steel is a high-performance high speed steel which exhibits superior hot (red) hardness compared to T15 and M42 high speed steels, and wear resistance comparable to tha..
Critical Temperature 838 °C
1540 °F
Crucible Steel HALCOMB® 425 Tool Steel, AISI H19
Halcomb 425 is designed for higher operating temperatures than H13, where wear resistance and heat check resistance are more critical than toughness. While H19 has excellent heat checking resistance..
Critical Temperature 838 °C
1540 °F
Ac1
Latrobe DuraTech™ A11 Powder Metal Tool Steel (AISI A11)
DuraTech A11 powder metal tool steel a versatile air-hardening tool and die steel which provides extremely high wear resistance in combination with relatively high impact toughness. A very large vol..
Critical Temperature 838 °C
1540 °F
Ac3
Latrobe LSS™ S7 Shock-Resisting Tool Steel (ASTM S7)
TLS S7 Shock-Resisting tool steel is an air or oil hardening tool steel that is characterized by very high impact toughness. The combination of strength and high toughness makes S7 tool steel a cand..
Critical Temperature 838 °C
1540 °F
Ar1
Latrobe LSS™ H21 Hot Work Tool Steel (ASTM H21)
TLS H21 hot work tool steel is a low-carbon, tungsten hot work steel that exhibits excellent resistance to softening at elevated temperature. This grade is intended for elevated-temperature service ..
Copyright © lookpolymers.com All Rights Reserved