Polymer Property : CTE, linear = 5.950 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 10.71 µm/m-°C

@Temperature 21.0 - 100 °C
5.950 µin/in-°F

@Temperature 69.8 - 212 °F
Latrobe DuraTechâ„¢ NINE Powder Metal Tool Steel
DuraTech NINE is an air-hardening, powder metal tool steel that provides very high wear resistance in combination with high impact toughness. A large volume of hard vanadium carbides provides the hi..
CTE, linear 10.71 µm/m-°C

@Temperature 21.0 - 100 °C
5.950 µin/in-°F

@Temperature 69.8 - 212 °F
Latrobe DuraTech™ A11 Powder Metal Tool Steel (AISI A11)
DuraTech A11 powder metal tool steel a versatile air-hardening tool and die steel which provides extremely high wear resistance in combination with relatively high impact toughness. A very large vol..