Material Notes:
Description: LUTENE XL2700BK has excellent strippability, processability, weather resistance, heat resistance for medium and high voltage power cables. The advantage of LUTENE XL2700BK over conventional strippable insulation shield compounds include: 1) Consistent, clean adhesion level over -40 to 70°C temperature range. 2) Excellent extruded surface smoothness, with fewer and smaller surface protrusions over broad range of shear rates.Applications: Insulation shielding of medium and high voltage cableInformation provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D1505
pH 6.0 - 7.0
6.0 - 7.0
Mechanical Properties Metric English Comments
Tensile Strength at Break 14.8 MPa
2150 psi
ASTM D638
14.06 MPa

@Temperature 121 °C,
Time 605000 sec
2039 psi

@Temperature 250 °F,
Time 168 hour
ASTM D638
Elongation at Break 250 %
250 %
ASTM D638
225 %

@Temperature 121 °C,
Time 605000 sec
225 %

@Temperature 250 °F,
Time 168 hour
ASTM D638
Thermal Properties Metric English Comments
Melting Point 110 - 130 °C
230 - 266 °F
Brittleness Temperature <= -50.0 °C
<= -58.0 °F
ASTM D746
Electrical Properties Metric English Comments
Volume Resistivity 300 ohm-cm

@Temperature 23.0 °C
300 ohm-cm

@Temperature 73.4 °F
ASTM D257
800 ohm-cm

@Temperature 90.0 °C
800 ohm-cm

@Temperature 194 °F
ASTM D257