Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 14.06 MPa @Temperature 121 °C, Time 605000 sec |
2039 psi @Temperature 250 °F, Time 168 hour |
ASTM D638 |
LG Chemical LUTENE XL2700BK PE Compound Description: LUTENE XL2700BK has excellent strippability, processability, weather resistance, heat resistance for medium and high voltage power cables. The advantage of LUTENE XL2700BK over conventi.. |