Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Volume Resistivity = 800 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 800 ohm-cm

@Temperature 90.0 °C
800 ohm-cm

@Temperature 194 °F
ASTM D257
LG Chemical LUTENE XL2700BK PE Compound
Description: LUTENE XL2700BK has excellent strippability, processability, weather resistance, heat resistance for medium and high voltage power cables. The advantage of LUTENE XL2700BK over conventi..
Volume Resistivity 800 ohm-cm

@Temperature 90.0 °C
800 ohm-cm

@Temperature 194 °F
ASTM D257
LG Chemical LUTENE XL2808BK PE Compound
Description: LUTENE XL2808BK has an excellent electrical properties and assists in obtaining a minimum shrink back on aluminum conductor, especially solid conductor. LUTENE XL2808BK is specifically ..
Copyright © lookpolymers.com All Rights Reserved