Lucobit Lucofin® 1492 Chemically Modified Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , Anhydride-Modified Polyethylene
Manufacturer Lucobit AG
Trade Name Lucofin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucobit Lucofin® 1492 Chemically Modified Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lucofin® 1492 is a chemically modified polyethylene, i.e. EBA grafted with maleic anhydride (MA). Lucofin® 1492 can be used pure or as a component in mixtures applications where improved polarity is required.Information provided by Lucobit AG
Physical Properties Metric English Comments
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Processing Properties Metric English Comments
Processing Temperature 160 - 270 °C
320 - 518 °F
Extrusion